Material Number | Material Number (single) | Standard | Range of Application | Standard Status | Country | Predecessor | Remark | Application temperature [°C] |
---|---|---|---|---|---|---|---|---|
1.4471 (SEW 410 : 2017-12) | 1.4471 | SEW 410 : 2017-12 | Supersedes SEW 410 : 1998-07 | Valid | Germany | GX3CrNiMoWCuN27-6-3-1 | Castings with high resistance to pitting and crevice corrosion and to intergranular corrosion in chloride and fluoride media, e.g. for flue gas desulphurization systems (plants), injection water with H2S. | ≤ 280 |
Chemical Composition
C [%] | Cr [%] | Cu [%] | Mn [%] | Mo [%] | N [%] | Ni [%] | P [%] | S [%] | Si [%] | W [%] | Source |
---|---|---|---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur | blur |
Mechanical Properties
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Tensile Strength [MPa] | Yield Strength (0.2% offset) [MPa] | Elongation A [%] | Source | Remark |
---|---|---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur | blur | blur |
Physical Properties
Temperature [°C] | Density [g/cm³] | Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] | Thermal Conductivity [W/(m*K)] | Mean Specific Heat Capacity [kJ/(kg*K)] | Linear Shrinkage [%] | Source |
---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur |
blur | blur | blur | blur | blur | blur | blur |
Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]
Exclusive Insight Locked!
This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.
Unlock NowWelding and Joining
Welding and Joining - Evaluation | Preheating [°C] | Interpass Temperature [°C] | Added Materials | Source | Remark |
---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur |
Toughness Data (Impact)
Semi-finished Product | Condition | Nominal Size [mm] | Temperature [°C] | Specimen Shape | Notch Impact Energy [J] | Source |
---|---|---|---|---|---|---|
blur | blur | blur | blur | blur | blur | blur |
Heat Treatment
Heat Treatment | Temperature [°C] | Medium | Source |
---|---|---|---|
blur | blur | blur | blur |
Producer/Supplier/Trade names
Tradename | Supplier |
---|---|
G 4471 | Dörrenberg Edelstahl GmbH, Engelskirchen |
1.4471 | Klaus Kuhn Edelstahlgießerei GmbH, Radevormwald |
Guronit MA 26/6 RW | SCHMOLZ + BICKENBACH GUSS GmbH, Krefeld |
DUX G 4471 | SCHMOLZ + BICKENBACH GUSS GmbH, Krefeld |
Märker G 4471 | Schmidt + Clemens GmbH + Co. KG, Edelstahlwerk Kaiserau, Lindlar |
Material Compliance
REACh | RoHS |
---|---|