CuSn7Pb15-C | CC496K Material Datasheet - Properties - Materials Portal

CuSn7Pb15-C | CC496K Material Datasheet

Unlock Exclusive Materials Data

Gain access to a wealth of materials data by joining our Materials Portal.

Register for Free or Upgrade for Full Access

Material Description

Material NumberMaterial Number (single)StandardRange of ApplicationStandard StatusCountryPredecessorRemark
CC496K (DIN EN 1982 : 2017-11) CC496K DIN EN 1982 : 2017-11Supersedes DIN EN 1982 : 2008-08ValidGermanyCuSn7Pb15-CCopper-tin-lead alloy castings.

Chemical Composition

Al [%]Cu [%]Fe [%]Mn [%]Ni [%]P [%]Pb [%]S [%]Sb [%]Si [%]Sn [%]Zn [%]SourceRemark
blurblurblurblurblurblurblurblurblurblurblurblurblurblur

Mechanical Properties

Casting MethodConditionDelivery Condition ENTemperature [°C]Tensile Strength [MPa]Yield Strength (0.2% offset) [MPa]Elongation A [%]Hardness HB | HBWSourceRemark
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblur

Physical Properties

ConditionTemperature [°C]Melting Temperature [°C]Density [g/cm³]Young's Modulus [GPa]Mean Coefficient of Thermal Expansion [10^-6*K^-1]Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1]Thermal Conductivity [W/(m*K)]Linear Shrinkage [%]Electric Conductivity [MS/m]Specific Electric Conductivity [% IACS]Source
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur
blurblurblurblurblurblurblurblurblurblurblurblur

Young's Modulus [GPa] vs Temperature [°C]

Exclusive Insight Locked!

This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.

Unlock Now

Mean Coefficient of Thermal Expansion (reference 20°C) [10^-6*K^-1] vs Temperature [°C]

Exclusive Insight Locked!

This premium diagram is currently blurred. Gain full access to detailed insights and stay ahead with exclusive content.

Unlock Now

Cross Reference

Material NameCountryStandardSource
G-CuPb15SnGermanyDIN 1716 DIN CEN/TS 13388 (DIN SPEC 9700)
2.1182.01GermanyDIN 1716 DIN CEN/TS 13388 (DIN SPEC 9700)
GZ-CuPb15SnGermanyDIN 1716 DIN CEN/TS 13388 (DIN SPEC 9700)
2.1182.03GermanyDIN 1716 DIN CEN/TS 13388 (DIN SPEC 9700)
GC-CuPb15SnGermanyDIN 1716 DIN CEN/TS 13388 (DIN SPEC 9700)
2.1182.04GermanyDIN 1716 DIN CEN/TS 13388 (DIN SPEC 9700)
CuSn7Pb15-CEuropeEN 1982 
CuPb15Sn8InternationalISO 1338Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
CAC604JapanJIS H 5120Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
LBC4JapanJIS H 5115Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
Cu Sn7 Pb15NorwayDNV 
Leaded bronzeNorwayDNV 
B271 UNS C93800USAASTM B271Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
B505 UNS C93800USAASTM B505Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
B584 UNS C93800USAASTM B584Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
B66 UNS C93800USAASTM B66Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
B763 UNS C93800USAASTM B763Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf
C93800USAUNSDeutsches Kupferinstitut Berufsverband e.V., Düsseldorf
G-SnPbBz15Germany Deutsches Kupferinstitut Berufsverband e.V., Düsseldorf

Producer/Supplier/Trade names

TradenameSupplier
Bögra PS 138BÖGRA Technologie GmbH, Solingen
GC-CuPb15SnWieland Prometa GmbH, Düsseldorf
G-CuPb15SnCUMSAL GmbH, Wilnsdorf
DSt 157Dillenberg GmbH & Co, Düsseldorf
GC-CuPb15SnEd. Fitscher GmbH & Co KG, Oberhausen
CuSn7Pb15-CWieland Recycling GmbH, Ulm
GC-CuPb15SnMittelrheinische Metallgießerei H. Beyer GmbH & Co KG, Andernach
GC-CuPb15SnSchreier Metall GmbH, Erkrath
GC-CuPb15SnWieland-Werke AG, Ulm
Z 13ZOLLERN GmbH & Co. KG, Sigmaringen

Material Compliance

REAChRoHS